Alloy 46
Alloy 46 is obtained at a given temperature range by adjusting the content of nickel internal energy and the expansion coefficient of different soft glass and ceramic matching a series of expansion alloy, its expansion coefficient and the Curie temperature increases with the increase of nickel content.The assembly is widely used in electric vacuum industry the sealing structure of the material.
Chemical Composition in %, Invar
Ni | Fe | C | P | Si | Co | Mn | Al | S |
---|---|---|---|---|---|---|---|---|
- | - | ≤ | ≤ | ≤ | ≤ | ≤ | ≤ | ≤ |
45.0~47.0 | Bal | 0.05 | 0.02 | 0.3 | - | 0.80 | 0.10 | 0.02 |
Basic physical constants and mechanical properties of the alloy:
Brand | Thermal conductivity | Specific heat capacity | Density | Electric resistivity | Curie point |
---|---|---|---|---|---|
Alloy 46 | 14.7 | 502J | 8.18 | 0.49 | 420 |
Typical expansion character(10 -6 / ºC )
Temperature range | 20~100 | 20~200 | 20~300 | 20~350 | 20~400 | 20~450 | 20~500 | 20~600 |
---|---|---|---|---|---|---|---|---|
Expansion coefficient | 7.5 | 7.5 | 7.1 | 7.1 | 7.2 | 7.1 | 8.3 | 9.5 |
Alloy 46 is used mainly for precision impedance diaphragm, with synthetic sapphire, soft glass, ceramic sealing.